{"id":3074,"date":"2026-11-22T16:41:18","date_gmt":"2026-11-22T16:41:18","guid":{"rendered":"https:\/\/hscodematch.com\/news\/tanzania-drafts-five-paint-and-lacquer-standards-with-90-ppm-lead\/"},"modified":"2026-11-22T16:41:19","modified_gmt":"2026-11-22T16:41:19","slug":"tanzania-drafts-five-paint-and-lacquer-standards-with-90-ppm-lead","status":"publish","type":"post","link":"https:\/\/hscodematch.com\/news\/tanzania-drafts-five-paint-and-lacquer-standards-with-90-ppm-lead\/","title":{"rendered":"Tanzania Drafts Five Paint and Lacquer Standards With 90 ppm Lead Limit"},"content":{"rendered":"\n<p class=\"wp-block-paragraph hsn-lede\">Tanzania has introduced five new technical specifications for <strong>solvent-based coatings, primers, and industrial paints<\/strong> under CHDC 13 standards, addressing quality and performance requirements across multiple product categories.<\/p>\n<p class=\"wp-block-paragraph\">The Tanzania Bureau of Standards (TBS) has issued five draft standards for solvent-based paints, primers, sealers and lacquers sold in Tanzania.<\/p>\n<p class=\"wp-block-paragraph\">The drafts cover paint for pre-painted metal sheets, primer for the same sheets, chalkboard-style paint, a wood sealer and a furniture lacquer. Each one sets quality tests, a lead limit and label rules<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\" id=\"hsn-cite-1\">1<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">In short, a can of these coatings will need to pass set laboratory tests and carry a full label. Every one of the five products must contain <strong>no more than 90 ppm of lead<\/strong>, which means 90 parts per million<sup class=\"hsn-cite\"><a href=\"#hsn-ref-2\" id=\"hsn-cite-2\">2<\/a><\/sup>.<\/p>\n<h2 class=\"wp-block-heading\">Which paints and lacquers do the Tanzania drafts cover?<\/h2>\n<p class=\"wp-block-paragraph\">TBS, Tanzania&#8217;s national standards body, set up under the Standards Act Cap. 130, wrote all five drafts<sup class=\"hsn-cite\"><a href=\"#hsn-ref-3\" id=\"hsn-cite-3\">3<\/a><\/sup>. Its Paints and Varnish Technical Committee, known as CDC 13, prepared them under the Chemical Divisional Standards Committee<sup class=\"hsn-cite\"><a href=\"#hsn-ref-3\">3<\/a><\/sup>.<\/p>\n<figure class=\"hsn-fig hsn-fig--solid hsn-fig--v2\" data-at=\"which-paints-and-lacquers-do-the-tanzania-drafts-cover\">\n  <div class=\"hsn-fig__table\">\n    <h4>The five draft Tanzania paint standards<\/h4>\n    <div class=\"pcrstb-wrap\"><table>\n      <thead>\n        <tr><th>Draft<\/th><th>Product covered<\/th><\/tr>\n      <\/thead>\n      <tbody>\n        <tr><th>CHDC 13 (4990)<\/th><td>Solvent-based paint for coil coatings<\/td><\/tr>\n        <tr><th>CHDC 13 (4991)<\/th><td>Solvent-based primer for coil coatings<\/td><\/tr>\n        <tr><th>CHDC 13 (4993)<\/th><td>Nitrocellulose sanding sealer for wood<\/td><\/tr>\n        <tr><th>CHDC 13 (4994)<\/th><td>Board paint for writing boards<\/td><\/tr>\n        <tr><th>CHDC 13 (4995)<\/th><td>Bright acid-catalysed interior furniture lacquer<\/td><\/tr>\n      <\/tbody>\n    <\/table><\/div>\n  <\/div>\n<\/figure>\n<p class=\"wp-block-paragraph\">The five drafts are:<\/p>\n<ul>\n<li><strong>Solvent-based paint for coil coatings<\/strong>, CHDC 13 (4990). This covers the back coats and topcoats painted onto metal sheets at the factory<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/li>\n<li><strong>Solvent-based primer for coil coatings<\/strong>, CHDC 13 (4991). This covers the first layer painted onto metal sheets or strips used in building work<sup class=\"hsn-cite\"><a href=\"#hsn-ref-2\">2<\/a><\/sup>.<\/li>\n<li><strong>Nitrocellulose sanding sealer<\/strong>, CHDC 13 (4993). This is a wood coating that seals the surface before the final finish<sup class=\"hsn-cite\"><a href=\"#hsn-ref-4\" id=\"hsn-cite-4\">4<\/a><\/sup>.<\/li>\n<li><strong>Board paint<\/strong>, CHDC 13 (4994). This is paint for writing boards and for wooden, metal and concrete surfaces<sup class=\"hsn-cite\"><a href=\"#hsn-ref-3\">3<\/a><\/sup>.<\/li>\n<li><strong>Bright acid-catalysed interior furniture lacquer<\/strong>, CHDC 13 (4995). This is a clear or tinted, fast-drying lacquer for indoor furniture<sup class=\"hsn-cite\"><a href=\"#hsn-ref-5\" id=\"hsn-cite-5\">5<\/a><\/sup>.<\/li>\n<\/ul>\n<p class=\"wp-block-paragraph\">Each document is marked as a draft Tanzania standard and a first edition, dated 2026<sup class=\"hsn-cite\"><a href=\"#hsn-ref-4\">4<\/a><\/sup>. &quot;Coil coating&quot; means paint applied to rolled metal sheet in a factory line, before the sheet is cut and shaped.<\/p>\n<p class=\"wp-block-paragraph\">&quot;Solvent-based&quot; means the paint is thinned with a chemical liquid rather than water. All five drafts carry the same international standards class number for paints, 87.040<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/p>\n<h2 class=\"wp-block-heading\">What does the lead limit mean for paint shipments?<\/h2>\n<p class=\"wp-block-paragraph\">The single rule shared by all five drafts is a ceiling on lead. The coil paint, primer, sealer, board paint and lacquer each have a <strong>maximum total lead content of 90 ppm<\/strong><sup class=\"hsn-cite\"><a href=\"#hsn-ref-5\">5<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">Laboratories must measure lead with Tanzania standard TZS 1894. This method burns the sample in a flame and reads the lead it gives off<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">For a seller, this means a test report on lead will matter for every batch of these coatings. A product made with lead-based pigments or driers would fail the limit.<\/p>\n<h2 class=\"wp-block-heading\">What tests must coil coating paint pass?<\/h2>\n<p class=\"wp-block-paragraph\">The coil coating paint draft is the longest of the five. It splits the paint into three kinds: the <strong>back coat<\/strong>, also called bottom coat, the standard topcoat and the durable topcoat<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">Paint in the can must be even, with no hard lumps after stirring. The dried film must have one colour and a smooth surface, with no bubbles or holes<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">The draft then sets a table of 16 tests. The main ones are:<\/p>\n<ul>\n<li><strong>Solids content<\/strong>: at least 55% by mass for back coats. For topcoats it is 60% for white and light colours, 50% for other colours, 45% for metallic-effect paints and 40% for clear coats<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/li>\n<li><strong>Resistance to solvent rubbing<\/strong>: at least 50 rub cycles for back coats and effect paints, and 100 for other topcoats<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/li>\n<li><strong>Impact strength<\/strong>: the coated sheet must survive a falling weight of at least 60 kg\u00b7cm on back coats and 90 kg\u00b7cm on topcoats<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/li>\n<li><strong>Bending<\/strong>: a T-bend result of 4T for back coats and 3T for topcoats. This tests whether paint cracks when the sheet is folded<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/li>\n<li><strong>Curing<\/strong>: baking at 200 to 300 \u00b0C for 20 to 50 seconds<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/li>\n<\/ul>\n<p class=\"wp-block-paragraph\">Topcoats face extra tests that back coats do not. They must resist scratching under a load of at least 1,200 grams<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>. They must also show no damage after 24 hours in a 5% acid solution and a 5% alkali solution<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/p>\n<h2 class=\"wp-block-heading\">How long must outdoor coil paint resist salt and sunlight?<\/h2>\n<p class=\"wp-block-paragraph\">The draft sets longer test times for the durable topcoat than for the standard one. In the salt spray test, a rust test, the standard topcoat runs for <strong>240 hours<\/strong> and the durable topcoat for <strong>480 hours<\/strong><sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/p>\n<figure class=\"hsn-fig hsn-fig--solid hsn-fig--v2\" data-at=\"how-long-must-outdoor-coil-paint-resist-salt-and-sunlight\">\n    <div class=\"hsn-fig__chart\">\n    <h4>Durable topcoat test times, hours<\/h4>\n    <div class=\"hsn-fig__bar\" data-series=\"1\">\n      <span class=\"hsn-fig__lab\">Xenon lamp<\/span>\n      <span class=\"hsn-fig__bartrack\"><span class=\"hsn-fig__barfill\" data-v=\"100\"><\/span><\/span>\n      <span class=\"hsn-fig__num\">1,500 h<\/span>\n    <\/div>\n    <div class=\"hsn-fig__bar\" data-series=\"2\">\n      <span class=\"hsn-fig__lab\">UVA-340 lamp<\/span>\n      <span class=\"hsn-fig__bartrack\"><span class=\"hsn-fig__barfill\" data-v=\"50\"><\/span><\/span>\n      <span class=\"hsn-fig__num\">720 h<\/span>\n    <\/div>\n    <div class=\"hsn-fig__bar\" data-series=\"3\">\n      <span class=\"hsn-fig__lab\">Salt spray<\/span>\n      <span class=\"hsn-fig__bartrack\"><span class=\"hsn-fig__barfill\" data-v=\"30\"><\/span><\/span>\n      <span class=\"hsn-fig__num\">480 h<\/span>\n    <\/div>\n    <div class=\"hsn-fig__bar\" data-series=\"4\">\n      <span class=\"hsn-fig__lab\">UVB-313 lamp<\/span>\n      <span class=\"hsn-fig__bartrack\"><span class=\"hsn-fig__barfill\" data-v=\"25\"><\/span><\/span>\n      <span class=\"hsn-fig__num\">400 h<\/span>\n    <\/div>\n  <\/div><\/figure>\n<p class=\"wp-block-paragraph\">After that time, slight colour change is allowed. Rusting, cracking and peeling are not allowed, and blistering must stay at grade 2 or below<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">Paint for outdoor use must also pass light tests under laboratory lamps:<\/p>\n<ul>\n<li><strong>UVA-340 lamp<\/strong>: 500 hours for standard topcoats and 720 hours for durable topcoats<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/li>\n<li><strong>UVB-313 lamp<\/strong>: 200 hours for standard topcoats and 400 hours for durable topcoats<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/li>\n<li><strong>Xenon lamp<\/strong>: 800 hours for standard topcoats and 1,500 hours for durable topcoats<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/li>\n<\/ul>\n<p class=\"wp-block-paragraph\">After each test the colour change must be grade 2 or less, and chalking grade 1 or less. Chalking is the powder that forms on old paint<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>. The xenon test also limits the loss of gloss to grade 2<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">These tests use methods of the International Organization for Standardization (ISO), including ISO 9227 for salt spray and ISO 16474 for the lamps<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>. The draft lists an industry standard for coil coatings, HG\/T 2820\u20142026, in its reading list<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>.<\/p>\n<h2 class=\"wp-block-heading\">What does the coil coating primer draft require?<\/h2>\n<p class=\"wp-block-paragraph\">The primer draft is shorter. It applies to primers used on metal sheets or strips for building work, applied by the coil-coating process<sup class=\"hsn-cite\"><a href=\"#hsn-ref-2\">2<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">The primer must suit the metal, its pre-treatment and the layers painted on top. It must be even and free of hard lumps after stirring<sup class=\"hsn-cite\"><a href=\"#hsn-ref-2\">2<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">The draft sets three tests in its table:<\/p>\n<ul>\n<li><strong>Solids content<\/strong>: at least 45% by mass<sup class=\"hsn-cite\"><a href=\"#hsn-ref-2\">2<\/a><\/sup>.<\/li>\n<li><strong>Fineness of grind<\/strong>: no more than 30 micrometres. This measures how finely the pigment is ground<sup class=\"hsn-cite\"><a href=\"#hsn-ref-2\">2<\/a><\/sup>.<\/li>\n<li><strong>Lead<\/strong>: no more than 90 ppm<sup class=\"hsn-cite\"><a href=\"#hsn-ref-2\">2<\/a><\/sup>.<\/li>\n<\/ul>\n<h2 class=\"wp-block-heading\">What are the rules for board paint and wood sealer?<\/h2>\n<p class=\"wp-block-paragraph\">Board paint is paint that gives a surface for writing or marking, which can then be cleaned<sup class=\"hsn-cite\"><a href=\"#hsn-ref-3\">3<\/a><\/sup>. It must be suitable for brush, roller or spray<sup class=\"hsn-cite\"><a href=\"#hsn-ref-3\">3<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">The board paint draft sets these limits<sup class=\"hsn-cite\"><a href=\"#hsn-ref-3\">3<\/a><\/sup>:<\/p>\n<ul>\n<li>Solids content of 57% by mass, plus or minus 2.<\/li>\n<li>Specific gravity, a measure of weight against water, of at least 1.2.<\/li>\n<li><strong>Surface-drying time of 3 to 4 hours<\/strong> and hard-drying time of 24 hours.<\/li>\n<li>A flash point of 38.0 \u00b0C. This is the temperature at which the paint&#8217;s vapour can catch fire.<\/li>\n<\/ul>\n<p class=\"wp-block-paragraph\">The nitrocellulose sanding sealer is a one-component wood coating. It fills pores and small marks so the wood can be sanded before the final coat<sup class=\"hsn-cite\"><a href=\"#hsn-ref-4\">4<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">The sealer draft requires solids of 30% by mass, plus or minus 2. Its specific gravity must be 0.93 to 0.95<sup class=\"hsn-cite\"><a href=\"#hsn-ref-4\">4<\/a><\/sup>. It must be <strong>touch-dry in 45 to 60 minutes<\/strong> and ready for sanding in 4 to 6 hours<sup class=\"hsn-cite\"><a href=\"#hsn-ref-4\">4<\/a><\/sup>.<\/p>\n<h2 class=\"wp-block-heading\">How must the furniture lacquer perform?<\/h2>\n<p class=\"wp-block-paragraph\">The furniture lacquer is a two-component product. The lacquer is mixed with a catalyst, a chemical that makes it harden<sup class=\"hsn-cite\"><a href=\"#hsn-ref-5\">5<\/a><\/sup>.<\/p>\n<figure class=\"hsn-fig hsn-fig--solid hsn-fig--v2\" data-at=\"how-must-the-furniture-lacquer-perform\">\n  <div class=\"hsn-fig__table\">\n    <h4>Furniture lacquer requirements<\/h4>\n    <div class=\"pcrstb-wrap\"><table>\n      <thead>\n        <tr><th>Requirement<\/th><th>Limit<\/th><\/tr>\n      <\/thead>\n      <tbody>\n        <tr><th>Solids content<\/th><td>At least 43% by mass<\/td><\/tr>\n        <tr><th>Specific gravity<\/th><td>0.90 to 1.0<\/td><\/tr>\n        <tr><th>Touch-dry time<\/th><td>15 to 20 minutes<\/td><\/tr>\n        <tr><th>Pot life<\/th><td>24 hours<\/td><\/tr>\n        <tr><th>Lead<\/th><td>No more than 90 ppm<\/td><\/tr>\n      <\/tbody>\n    <\/table><\/div>\n  <\/div>\n<\/figure>\n<p class=\"wp-block-paragraph\">It must be clear or tinted and suitable for spraying. The finish must be glossy, eggshell or matt, as the maker declares<sup class=\"hsn-cite\"><a href=\"#hsn-ref-5\">5<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">The draft sets these limits<sup class=\"hsn-cite\"><a href=\"#hsn-ref-5\">5<\/a><\/sup>:<\/p>\n<ul>\n<li><strong>Solids content of at least 43%<\/strong> by mass.<\/li>\n<li>Specific gravity of 0.90 to 1.0.<\/li>\n<li>Touch-dry time of 15 to 20 minutes.<\/li>\n<li>A pot life of 24 hours. Pot life is the time the mixed lacquer stays usable.<\/li>\n<\/ul>\n<p class=\"wp-block-paragraph\">An annex explains how to test pot life. The mixed lacquer is kept at 27 \u00b0C, plus or minus 2, and its thickness is measured every hour<sup class=\"hsn-cite\"><a href=\"#hsn-ref-5\">5<\/a><\/sup>. The pot life ends when the lacquer turns to gel, becomes stringy or can no longer be thinned<sup class=\"hsn-cite\"><a href=\"#hsn-ref-5\">5<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">For test panels, the lacquer and catalyst are mixed at <strong>4% catalyst by volume<\/strong>, unless the maker declares and checks another ratio<sup class=\"hsn-cite\"><a href=\"#hsn-ref-5\">5<\/a><\/sup>.<\/p>\n<h2 class=\"wp-block-heading\">What must the labels on paint cans show?<\/h2>\n<p class=\"wp-block-paragraph\">Every draft has a label rule. Each package must be labelled clearly and permanently in <strong>English, Kiswahili or both<\/strong><sup class=\"hsn-cite\"><a href=\"#hsn-ref-3\">3<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">All five drafts require the label to show<sup class=\"hsn-cite\"><a href=\"#hsn-ref-4\">4<\/a><\/sup>:<\/p>\n<ul>\n<li>the product name;<\/li>\n<li>the maker&#8217;s name and physical address;<\/li>\n<li>the net content;<\/li>\n<li>the batch or lot number;<\/li>\n<li>the date of manufacture;<\/li>\n<li>an expiry or best-before date, or the shelf life;<\/li>\n<li>instructions for use, storage and disposal;<\/li>\n<li>safety warnings and hazard symbols.<\/li>\n<\/ul>\n<p class=\"wp-block-paragraph\">Some products need more. The furniture lacquer label must give the mixing ratio, the catalyst, drying and recoating times and the pot life<sup class=\"hsn-cite\"><a href=\"#hsn-ref-5\">5<\/a><\/sup>. The sealer label must give drying, sanding and recoating times<sup class=\"hsn-cite\"><a href=\"#hsn-ref-4\">4<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">The coil paint label must say whether the paint is a standard or durable type, and give curing instructions<sup class=\"hsn-cite\"><a href=\"#hsn-ref-1\">1<\/a><\/sup>. The primer label must include fire warnings<sup class=\"hsn-cite\"><a href=\"#hsn-ref-2\">2<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">Every draft also requires well-sealed containers that protect the paint and do not react with it<sup class=\"hsn-cite\"><a href=\"#hsn-ref-2\">2<\/a><\/sup>. Samples for testing are taken under TZS 524, the Tanzania version of ISO 15528<sup class=\"hsn-cite\"><a href=\"#hsn-ref-3\">3<\/a><\/sup>.<\/p>\n<h2 class=\"wp-block-heading\">Who is affected by the Tanzania paint standards?<\/h2>\n<p class=\"wp-block-paragraph\">Paint makers abroad that ship these five products to Tanzania will be the most affected. Their products will need to meet the test limits and the lead ceiling, and their labels will need the listed details.<\/p>\n<p class=\"wp-block-paragraph\">Importers and distributors in Tanzania will need to check labels in English or Kiswahili before goods go on shelves. Makers of steel roofing and cladding sheets use coil paints and primers, so the coil drafts reach them too.<\/p>\n<p class=\"wp-block-paragraph\">Furniture workshops and joiners buy sealers and lacquers. School and office suppliers buy board paint.<\/p>\n<h2 class=\"wp-block-heading\">What happens next for the draft standards?<\/h2>\n<p class=\"wp-block-paragraph\">The documents are still drafts, and none of them gives a start date.<\/p>\n<p class=\"wp-block-paragraph\">Each draft says Tanzania standards are reviewed to keep pace with science and technology<sup class=\"hsn-cite\"><a href=\"#hsn-ref-4\">4<\/a><\/sup>. Each one was published under the authority of the TBS Board of Directors<sup class=\"hsn-cite\"><a href=\"#hsn-ref-5\">5<\/a><\/sup>.<\/p>\n<p class=\"wp-block-paragraph\">The draft files are held on the document site of the World Trade Organization (WTO) for technical barriers to trade, the WTO&#8217;s system for product rules<sup class=\"hsn-cite\"><a href=\"#hsn-ref-2\">2<\/a><\/sup>. Final versions may differ from the drafts once TBS adopts them.<\/p>\n<h2 class=\"wp-block-heading\">Key points on Tanzania&#8217;s draft paint standards<\/h2>\n<p class=\"wp-block-paragraph\">The table gives the main facts from the five drafts.<\/p>\n<div class=\"hsn-table\">\n<div class=\"pcrstb-wrap\"><table>\n<thead><tr><th>Question<\/th><th>Answer<\/th><\/tr><\/thead>\n<tbody>\n<tr><td>Who issued them?<\/td><td>Tanzania Bureau of Standards (TBS)<\/td><\/tr>\n<tr><td>How many drafts?<\/td><td>Five, all first editions<\/td><\/tr>\n<tr><td>Which goods?<\/td><td>Coil paint, coil primer, board paint, wood sealer, furniture lacquer<\/td><\/tr>\n<tr><td>Lead limit<\/td><td>90 ppm maximum for all five<\/td><\/tr>\n<tr><td>Coil topcoat salt spray<\/td><td>240 h standard, 480 h durable<\/td><\/tr>\n<tr><td>Primer solids<\/td><td>At least 45% by mass<\/td><\/tr>\n<tr><td>Lacquer pot life<\/td><td>24 hours<\/td><\/tr>\n<tr><td>Sealer touch-dry time<\/td><td>45 to 60 minutes<\/td><\/tr>\n<tr><td>Label language<\/td><td>English, Kiswahili or both<\/td><\/tr>\n<tr><td>Who must act?<\/td><td>Paint makers, exporters, importers<\/td><\/tr>\n<tr><td>Start date<\/td><td>Not yet set<\/td><\/tr>\n<\/tbody>\n<\/table><\/div>\n<\/div>\n<p class=\"wp-block-paragraph\">For now, the clearest effect is on lead. Any solvent-based paint, primer, sealer or lacquer in these five groups will need to test at 90 ppm of lead or less to meet the Tanzania drafts.<\/p>\n<h2 class=\"wp-block-heading hsn-refs-title\">Sources<\/h2>\n<ol class=\"hsn-refs\">\n<li id=\"hsn-ref-1\"><a class=\"hsn-refs__back\" href=\"#hsn-cite-1\" aria-label=\"Back to reference 1 in the text\">\u21a9<\/a> <a href=\"https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06021_00_e.pdf\" rel=\"noopener\" target=\"_blank\">26_06021_00_e.pdf<\/a> <span class=\"hsn-refs__url\">https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06021_00_e.pdf<\/span><\/li>\n<li id=\"hsn-ref-2\"><a class=\"hsn-refs__back\" href=\"#hsn-cite-2\" aria-label=\"Back to reference 2 in the text\">\u21a9<\/a> <a href=\"https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06022_00_e.pdf\" rel=\"noopener\" target=\"_blank\">26_06022_00_e.pdf<\/a> <span class=\"hsn-refs__url\">https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06022_00_e.pdf<\/span><\/li>\n<li id=\"hsn-ref-3\"><a class=\"hsn-refs__back\" href=\"#hsn-cite-3\" aria-label=\"Back to reference 3 in the text\">\u21a9<\/a> <a href=\"https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06018_00_e.pdf\" rel=\"noopener\" target=\"_blank\">26_06018_00_e.pdf<\/a> <span class=\"hsn-refs__url\">https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06018_00_e.pdf<\/span><\/li>\n<li id=\"hsn-ref-4\"><a class=\"hsn-refs__back\" href=\"#hsn-cite-4\" aria-label=\"Back to reference 4 in the text\">\u21a9<\/a> <a href=\"https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06017_00_e.pdf\" rel=\"noopener\" target=\"_blank\">26_06017_00_e.pdf<\/a> <span class=\"hsn-refs__url\">https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06017_00_e.pdf<\/span><\/li>\n<li id=\"hsn-ref-5\"><a class=\"hsn-refs__back\" href=\"#hsn-cite-5\" aria-label=\"Back to reference 5 in the text\">\u21a9<\/a> <a href=\"https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06019_00_e.pdf\" rel=\"noopener\" target=\"_blank\">26_06019_00_e.pdf<\/a> <span class=\"hsn-refs__url\">https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06019_00_e.pdf<\/span><\/li>\n<\/ol>\n","protected":false},"excerpt":{"rendered":"<p>Tanzania has introduced five new technical specifications for solvent-based coatings, primers, and industrial paints under CHDC 13 standards, addressing\u2026<\/p>\n","protected":false},"author":1,"featured_media":3073,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"_lmt_disableupdate":"","_lmt_disable":"","_regnews_id":"36629","_hsn_citations":"[{\"n\":1,\"url\":\"https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06021_00_e.pdf\",\"label\":\"26_06021_00_e.pdf\"},{\"n\":2,\"url\":\"https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06022_00_e.pdf\",\"label\":\"26_06022_00_e.pdf\"},{\"n\":3,\"url\":\"https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06018_00_e.pdf\",\"label\":\"26_06018_00_e.pdf\"},{\"n\":4,\"url\":\"https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06017_00_e.pdf\",\"label\":\"26_06017_00_e.pdf\"},{\"n\":5,\"url\":\"https:\/\/members.wto.org\/crnattachments\/2026\/TBT\/TZA\/26_06019_00_e.pdf\",\"label\":\"26_06019_00_e.pdf\"}]","_hsn_no_sources":"","_hsn_content_hash":"639400239cf3ae760bae3d2919ad33a4951d8671:c6de59706e55e3619af7438a9eb6d2cbfdc14345","_yoast_wpseo_focuskw":"solvent-based paint and lacquer","footnotes":""},"categories":[149,15],"tags":[76],"class_list":["post-3074","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-africa","category-standards-conformity","tag-tanzania"],"_links":{"self":[{"href":"https:\/\/hscodematch.com\/news\/wp-json\/wp\/v2\/posts\/3074","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/hscodematch.com\/news\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/hscodematch.com\/news\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/hscodematch.com\/news\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/hscodematch.com\/news\/wp-json\/wp\/v2\/comments?post=3074"}],"version-history":[{"count":1,"href":"https:\/\/hscodematch.com\/news\/wp-json\/wp\/v2\/posts\/3074\/revisions"}],"predecessor-version":[{"id":3075,"href":"https:\/\/hscodematch.com\/news\/wp-json\/wp\/v2\/posts\/3074\/revisions\/3075"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/hscodematch.com\/news\/wp-json\/wp\/v2\/media\/3073"}],"wp:attachment":[{"href":"https:\/\/hscodematch.com\/news\/wp-json\/wp\/v2\/media?parent=3074"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/hscodematch.com\/news\/wp-json\/wp\/v2\/categories?post=3074"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/hscodematch.com\/news\/wp-json\/wp\/v2\/tags?post=3074"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}